Experimental values of coefficient of friction and wear depth.

Exp. no.COFWear (μm)

10.47856.2982
20.462767.1545
30.482038.055
40.399327.258
50.442388.0496
60.442159.0692
70.5260514.164
80.5498216.7608
90.5575122.0726
100.5242110.3106
110.5581111.789
120.5376714.6806
130.480666.9654
140.5154211.114
150.5644615.4086
160.4097614.8242
170.4588817.8212
180.4402720.0548
190.4082319.9342
200.4692624.2414
210.5041824.8034
220.4768511.6952
230.5185814.6608
240.4796716.5214
250.4236816.7828
260.5280620.4608
270.4661824.7724