Research Article

Preparation of Niobium Metal Powder by Two-Stage Magnesium Vapor Reduction of Niobium Pentoxide

Figure 3

Lateral cross-section of the niobium pellet (15 mm diameter) after reduced at 1123 K for 5 hours.