Research Article

Optimization of Conversion Treatment on Austenitic Stainless Steel Using Experimental Designs

Table 7

Doehlert design: results for each experiment.

No.Time
(s)
(°C)SS
(m²/m²)

130055.001200.85
218055.00720.78
327060.021340.86
421049.98590.73
527049.98860.75
621060.02940.83
724055.00990.81