Research Article

Mechanical Properties and Failure Topography of Banana Fiber PF Macrocomposites Fabricated by RTM and CM Techniques

Figure 2

Impact properties of banana fiber/PF composites at (a) different fiber lengths (fiber loading 30 wt%), (b) different fiber loadings (fiber length 30 mm).
936048.fig.002a
(a)
936048.fig.002b
(b)