Research Article

Mechanical Properties and Failure Topography of Banana Fiber PF Macrocomposites Fabricated by RTM and CM Techniques

Figure 3

SEM impact fractograph of 30 mm banana fiber/PF composite with 40 wt% fiber loading fabricated by (a) RTM and (b) CM techniques.