Research Article

Accumulative Roll Bonding of Pure Copper and IF Steel

Figure 9

Variation of microhardness after various ARB cycles: (a) IF steel preheated at 550°C and (b) pure copper preheated at 400°C.
179723.fig.009a
(a)
179723.fig.009b
(b)