Values of swelling exponent “n” and gel characteristic constant “k” for various samples studied.

Sample coden k × 103

A0.92310.60.975
B0.60938.90.986
C0.51760.10.978
D0.46533.00.987
E0.57324.60.988
F0.63328.00.974
G0.65687.70.988
H0.45571.10.992
I0.47265.60.985