Research Article

Influence of the Rate and Degree of Deformation on the Texture, Structure and Mechanical Properties of Steel

Figure 3

Inverse pole figures of steel after uniaxial tensile of 30% with varied deformation rate: (a) 0 mm/min (before tensile); (b) 0.1 mm/min; (c) 1 mm/min; (d) 60 mm/min; (e) 120 mm/min; (f) 300 mm/min.
397279.fig.003a
(a)
397279.fig.003b
(b)
397279.fig.003c
(c)
397279.fig.003d
(d)
397279.fig.003e
(e)
397279.fig.003f
(f)