Research Article

Effect of Coupling Agent on the Properties of Polymer/Date Pits Composites

Figure 3

SEM micrographs of the fracture surfaces of the Izod samples for the composites at 30 wt% date pits loading. Images were taken at low magnification (>100x), (a) HDPE/K, (b) HDPE/S, (c) PS100/K, and (d) PS100/S.
412432.fig.003a
(a)
412432.fig.003b
(b)
412432.fig.003c
(c)
412432.fig.003d
(d)