Review Article
Predicting and Preventing Flow Accelerated Corrosion in Nuclear Power Plant
Table 4
Possible variations in magnetite solubility dependency on hydrogen concentration.
|
Regiem | Hydrogen dependency | Reference |
| Normally | [H]1/3 | [53, 55, 56] | At high pHs above ~220°C | [H]−1/6 | [53, 55] | At temperatures below ~80–110°C | Independent | [55] | At high temperatures above pH~9.8 | Less than [H]1/3 | [55] |
|
|
Such effects could influence both dissolution and deposition.
|