Research Article

Characterization of Corrosive Bacterial Consortia Isolated from Water in a Cooling Tower

Figure 2

Tafel polarization curves of copper metal coupon in various systems after 10-day immersion in cooling water at 28°C: (a) control, (b) M. timonae ARTYP3, and (c) M. timonae ARTYP3 inoculated with biocide.