Research Article
Unidirectional Cordenka Fibre-Reinforced Furan Resin Full Biocomposite: Properties and Influence of High Fibre Mass Fraction
Figure 2
(a) SEM image of tensile fracture surface (51% FMF). (b) SEM image of tensile fracture surface (64% FMF). (c) SEM image of tensile fracture surface (75% FMF).
(a) |
(b) |
(c) |