Research Article
Experimental Investigations into Abrasive Waterjet Machining of Carbon Fiber Reinforced Plastic
Table 3
Results of experiments.
| Orientation | Kerf taper | Top delamination factor | Bottom delamination factor | Material removal rate | value | value | value | mm/mm | mm/mm | mm/mm | mm³/sec | m | m | m |
| 45 | 8.198 | 2.568075 | 0.7517 | 8.3782 | 6.576 | 15.168 | 77.9855 | 5.906 | 2.698575 | 0.83755 | 10.5438 | 6.794 | 13.248 | 74.1455 | 3.614 | 2.829075 | 0.9234 | 14.8598 | 7.012 | 10.048 | 67.7455 | 1.822 | 2.959575 | 1.00925 | 21.3262 | 7.23 | 5.568 | 58.7855 | 0.17 | 3.090075 | 1.0951 | 29.943 | 7.448 | 1.192 | 47.2655 |
| 60 | 13.022 | 3.2658 | 0.6296 | 6.9712 | 5.262 | 13.62 | 73.046 | 10.214 | 3.3963 | 0.6544 | 9.1368 | 5.48 | 11.7 | 69.206 | 7.406 | 3.5268 | 0.6792 | 13.4528 | 5.698 | 8.5 | 62.806 | 4.598 | 3.6573 | 0.704 | 19.9192 | 5.916 | 4.02 | 53.846 | 1.79 | 3.7878 | 0.7288 | 28.536 | 6.134 | 1.74 | 42.326 |
| 90 | 11.99 | 5.2593 | 0.3854 | 4.1572 | 2.634 | 13.953 | 75.236 | 8.15 | 5.3898 | 0.2881 | 6.3228 | 2.852 | 12.033 | 71.396 | 5.31 | 5.5203 | 0.1908 | 10.6388 | 3.07 | 8.833 | 64.996 | 2.47 | 5.6508 | 0.0935 | 17.1052 | 3.288 | 4.353 | 56.036 | 0.37 | 5.7813 | 0.0038 | 25.722 | 3.506 | 1.407 | 44.516 |
|
|