Review Article
A Review on Current Status of Stability and Knowledge on Liquid Electrolyte-Based Dye-Sensitized Solar Cells
Figure 11
(a) Comparison of cyclic voltamperometry recorded on Pt microelectrode for MPN-based electrolyte aged in contact with TiO2 during 100, 200, and 500 hours at 85°C/dark. (b) ATR-FT-IR spectra comparison of MPN-based reference electrolyte before and after 1000 hours ageing at 85°C/dark in contact with TiO2. (c) Quantification by LC/MS of NBB concentration as a function of ageing time at 85°C/dark in contact with TiO2.