Stretching frequencies of the carbonyl groupa for zirconium carboxylate complexes.

Sample (cm−1) (cm−1)
Asym.Sym.

Zr-115641439125
Zr-215601439121
Zr-316001466134
Zr-415851444141
Zr-515801428152
Zr-615561431125
Zr-715701425145
Zr-816151388227
Zr-915511381170
Zr-1016251351274