Conference Paper

Oxidation State of a Polyurethane Membrane after Plasma Etching

Figure 5

High resolution XPS spectrum of the N 1 s peak for PU membranes: (a) unetched and etched at 20 W for (b) 40 s and (c) 80 s.
347979.fig.005a
(a)
347979.fig.005b
(b)
347979.fig.005c
(c)