Research Article
Steam Explosion Pretreatment with Different Concentrations of Hydrogen Peroxide along with Citric Acid: A Former Step towards Bioethanol Production
Table 3
Cellulose crystallinity Index derived from XRD analysis.
| Different pretreated sample | Intensity at Iam | Intensity at I002 | CrI |
| Untreated biomass | 9.4 | 18.6 | 49.4 | 0.05% H2O2 | 10.3 | 24 | 57 | 0.1% H2O2 | 10.4 | 23.1 | 54.9 | 0.25% H2O2 | 10.26 | 22.7 | 54.8 | 0.5% H2O2 | 9.6 | 20.7 | 53.6 | 0.75% H2O2 | 10.7 | 22.8 | 53.07 | 1% H2O2 | 11.4 | 23.8 | 52.1 | 1 : 1 | 6.8 | 17.7 | 61.5 | 1 : 2 | 8.06 | 17.3 | 53.4 | 2 : 1 | 10.7 | 22.7 | 52.8 |
|
|