Research Article

Hot Corrosion Behaviour of Detonation Gun Sprayed Al2O3-40TiO2 Coating on Nickel Based Superalloys at 900°C

Figure 4

SEM micrographs of (a) Al2O3-40TiO2 coated Superni 718 (b) Al2O3-40TiO2 coated AE 435 (c) Superni 718 (d) AE 435 superalloys subjected to Na2SO4-82%Fe2(SO4)3 at 900°C for 50 cycles.
453607.fig.004a
(a)
453607.fig.004b
(b)
453607.fig.004c
(c)
453607.fig.004d
(d)