Hot Corrosion Behaviour of Detonation Gun Sprayed
Al2O3-40TiO2 Coating on Nickel Based Superalloys at 900°C
Table 3
Parameter used in Detonation Gun Spray.
| Parameters | Al2O3-40TiO2 coating |
| Oxygen flow rate (O2) | 4,800 SLPH | Pressure | 0.2 MPa | Acetylene flow rate (C2H2) | 1920 SLPH | Pressure | 0.14 MPa | Nitrogen flow rate (N2) | 800 SLPH | Pressure | 0.4 MPa | Spray angle | 90° | Spray distance | 200 mm | Power | 450 VA | Wire rate | 1–10 Hz | Coating thickness (average) | 250 m |
|
|