Research Article

Characterization of Defects and Stress in Polycrystalline Silicon Thin Films on Glass Substrates by Raman Microscopy

Figure 16

Variation of the intensities on the 2000 cm−1 and 2100 cm−1 LVMs with etching time. The intensity of both bands is normalized with the intensity at 0 s.
632139.fig.0016