Review Article

Degradable PHBHHx Modified by the Silk Fibroin for the Applications of Cardiovascular Tissue Engineering

Figure 1

Stress-strain curves of SF/PHBHHx films (a) and PHBHHx films (b) with a constant elongation rate of 5 mm/min. Four samples in the shape of rectangle in length × width × thickness of 4 0 × 5 × 0 . 1  mm were tested for each film [20].
389872.fig.001