Size of amino-MNPs at different parameters.

SampleParameterSize (nm):
𝑑 = diameter
Average size
 (nm)
NaOH (% w/v)Cycle

A-11.251ndnd
A-21.252ndnd
A-31.253 2 1 < 𝑑 < 1 1 3 47 ± 20
A-41.254 1 5 < 𝑑 < 5 3 33 ± 9

B-12.501ndnd
B-22.502 1 5 < 𝑑 < 1 2 3 45 ± 21
B-32.503 2 3 < 𝑑 < 1 0 7 43 ± 9
B-42.504 1 9 < 𝑑 < 7 6 41 ± 12

C-13.751ndnd
C-23.752 1 5 < 𝑑 < 6 9 29 ± 11
C-33.753 1 4 < 𝑑 < 9 2 43 ± 17
C-43.754 1 5 < 𝑑 < 6 9 39 ± 12

nd = not determined.