Composition of binder mixes (% by weight).
| Mix | CEM-I | Pouzzolane (PZ) | Slag (BFS) | Marble filler (MF) |
| 1 | 100 | 0 | 0 | 0 | 2 | 90 | 0 | 0 | 10 | 3 | 90 | 0 | 10 | 0 | 4 | 90 | 10 | 0 | 0 | 5 | 80 | 0 | 10 | 10 | 6 | 80 | 10 | 0 | 10 | 7 | 70 | 10 | 10 | 10 |
|
|