Research Article

Secondary Relaxation inside the Glass

Figure 2

Frequency of the maximum of the dielectric loss peak of secondary relaxation as a function of pressure at different temperatures (as indicated in the figure) for (a) PPGE, (b) PDE, (c) BMPC, (d) PPG400, (e) PVAc, (f) DGBEA.
764874.fig.002a
(a)
764874.fig.002b
(b)
764874.fig.002c
(c)
764874.fig.002d
(d)
764874.fig.002e
(e)
764874.fig.002f
(f)