Figure 6

Schematic of fractured surfaces in sintered clay samples showing crack lengths after thermal shock: (a) 63–90 μm, 𝑁 = 1 , 𝑎 = 1 . 3  mm; (b) 63–90 um, 𝑁 = 3 , 𝑎 = 2 . 5  mm; (c) 90–125 μm, 𝑁 = 1 , 𝑎 = 1 . 0  mm; (d) 90–125 μm, 𝑁 = 3 , 𝑎 = 1 . 5  mm.