Research Article
Preparation and Properties of Biodegradable Film Composites Using Modified Cellulose Fibre-Reinforced with PVA
Table 4
Oxygen permeation rate for ten different film composites.
| S. no. | Modified cellulose + PVA | OTR value; cc/sqm/day/atm |
| 1 | | 2005 | 2 | | 1907 | 3 | | 1854 | 4 | | 1701 | 5 | | 1589 | 6 | | 1498 | 7 | | 1245 | 8 | | 1087 | 9 | | 987 | 10 | | 843 |
|
|