Effect of Excess Silicon on the Formation of Ti3SiC2 Using Free Ti/Si/C Powders Synthesized via Arc Melting
Figure 3
FESEM morphology of sample ( = 0) scanned at (a) the dense surface and (b) pore site after arcing at a constant 90 A for 5 s.