Research Article
Effect of Plasma Surface Pretreatment on Ce3+-Doped GPTMS-ZrO2
Self-Healing Coatings on Aluminum Alloy
Table 1
fit data for the results obtained from potentiodynamic polarization measurements.
| Sample | (volts) | (A/cm2) | (ohms/cm2) |
| Bare Al-1 h | −0.772 | |
4291.2
| Bare Al-24 h | −0.788 | |
5517.4
| Al-GPZ-1 h | −0.838 | | | Al-GPZ-24 h | −0.781 | |
95159
| Al-GPZ-Ce-1 h | −0.824 | | | Al-GPZ-Ce-24 h | −0.818 | |
98225
| Al-GPZ-plasma-1 h | −0.819 | | | Al-GPZ-plasma-24 h | −0.754 | |
59109
| Al-GPZ-Ce-plasma-1 h | −0.802 | |
40135
| Al-GPZ-Ce-plasma-24 h | −0.761 | | |
|
|