Research Article

Electrochemical Synthesis of Nanocrystalline Ni0.5Zn0.5Fe2O4 Thin Film from Aqueous Sulfate Bath

Figure 7

Effect of annealing temperature on M-H hysteresis loops of Ni0.5Zn0.5Fe2O4 films. Annealing temperatures: (a) 800°C, (b) 850°C, and (c) 1000°C.
532168.fig.007