Research Article
Effect of Sliver Nanoparticles on Wool Fibre
Table 1
Tenacity of treated and untreated samples.
| Sample no. | Tenacity (gram/denier) Untreated sample | Tenacity (gram/denier) Treated sample |
| 1 | 1.33 | 1.99 | 2 | 1.12 | 1.84 | 3 | 1.32 | 1.90 | 4 | 1.08 | 1.69 | 5 | 0.90 | 1.52 |
|
|