Characteristics of Molecularly Imprinted Polymer Thin Layer for Bisphenol A and Response of the MIP-Modified Sensor

Figure 1

Photographs of BPA-MIP modified electrodes. (a) QCM electrode before MIP preparation. (b) The electrode after polymerization of MIP by UV irradiation for 2 min. (c) The electrode after polymerization of MIP by UV irradiation for 30 min. The black arrow indicates a crack in the MIP film.