Research Article

Processing and Properties of Nanocrystalline CoCrFeNiCuAlTiXVMo High Entropy Alloys by Mechanical Alloying

Figure 3

XRD patterns of equiatomic CoCrFeNiCuAlTiXVMo (X = Zn, Mn) HEA after 20 h of MA, heat-treated at 600°C for 1 h, and after HP.
167869.fig.003a
(a)
167869.fig.003b
(b)