Research Article

Potentiostatic Deposition and Characterization of Cuprous Oxide Thin Films

Figure 1

SEM photographs of thin films deposited at various deposition times: (a) 5, (b) 10, (c) 15, and (d) 30 min.
271545.fig.001a
(a)
271545.fig.001b
(b)
271545.fig.001c
(c)
271545.fig.001d
(d)