Evaluation of Preoxidized SUS304 as a Catalyst for Hydrocarbon Reforming

Table 1

Composition of SUS304 before and after oxidation at 1000°C for 2 h in O2 as measured by SEM-EDX.

ElementAtomic%OxideWeight%*
UnoxidizedOxidized

Cr20.0751.29 50.36
Fe73.1139.75 41.00
Ni6.828.96NiO8.64

Calculated from EDX data.