On the Failure and Fracture of Polymer Foam Containing Discontinuities
Figure 15
Quasi-static and dynamic fracture intensity factor as a function of initial crack length for A800 and A1200 foam (sample type 2).
We are committed to sharing findings related to COVID-19 as quickly as possible. We will be providing unlimited waivers of publication charges for accepted research articles as well as case reports and case series related to COVID-19. Review articles are excluded from this waiver policy. Sign up here as a reviewer to help fast-track new submissions.