Table 1
Composition of the used and rejuvenated bumpers.
| | Fraction soluble at 25°C % w/w | Fraction soluble at 75°C % w/w | Fraction soluble at 110°C % w/w | Cross-linked fraction % w/w | Inorganic fraction % w/w | Oxidable residue (carbon black % w/w |
| A, | 17 | 19 | 61 | tr | 1 | 2 | AR | 19 | 22 | 56 | tr | 1 | 2 | B | 11 | 31 | 40 | 1 | 15 | 2 | BR | 9 | 32 | 41 | 1 | 15 | 2 | C, | 9 | 30 | 47 | 1 | 12 | 1 | CR | 9 | 30 | 46 | 2 | 12 | 1 |
|
|
tr: traces.
|