Research Article

Corrosion Inhibition of Cu-Ni (90/10) Alloy in Seawater and Sulphide-Polluted Seawater Environments by 1,2,3-Benzotriazole

Figure 12

Cyclic voltammograms of Cu-Ni (90/10) alloy in synthetic seawater in the absence ((a): 1 h, (b): 48 h) and presence ((c): 1 h, (d): 48 h) of 3.33 mM BTAH. (Temperature: 30°C).
703929.fig.0012a
(a)
703929.fig.0012b
(b)
703929.fig.0012c
(c)
703929.fig.0012d
(d)