Research Article
A Study on the Adhesion of Styrene-Butadiene Rubber with Red Kaolinite on Aluminum Surface
Figure 8
Stress-strain of styrene-butadiene rubber adhesive with 50 wt% kaolinite at curing temperature of 200°C for period of time of 40 min.