Research Article

Corrosion Behavior of Zinc-Graphite Metal Matrix Composite in 1 M of HCl

Figure 7

Optical micrographs of the corroded surfaces of Zn/Graphite (3 wt.-%) MMCs after immersion in 1 M HCl solution for (a) 24 hr, (b) 48 hr, (c) 72 hr, and (d) 96 hr.
279856.fig.007a
(a)
279856.fig.007b
(b)
279856.fig.007c
(c)
279856.fig.007d
(d)