Research Article

Change in Surface Roughness of Esthetic Restorative Materials after Exposure to Different Immersion Regimes in a Cola Drink

Table 6

Showing mean difference in surface roughness ( , μm) and microhardness (HV) among various sub groups of group IV—composite resin (Filtek Z 350).

SubgroupSubgroupSurface roughness ( , m)
Mean difference ( value)Significance

Subgroup IVA (Control)Subgroup IVB−0.014>0.05NS
Subgroup IVC−0.018>0.05NS
Subgroup IVD−0.022>0.05NS
Subgroup IVE−0.029>0.05NS