Research Article

Functional Aromatic Poly(1,3,4-Oxadiazole-Ether)s with Benzimidazole Pendants: Synthesis, Thermal and Dielectric Studies

Figure 3

Plots of −Ln(ln(−1/)) versus 1/ × 10−3 for the decomposition step in the range 350–640°C of VALPOx, VALPOx-B-10, VALPOx-B-20, and VALPOx-B-30 polymer sample.