Enamel and Dentin Surface Finishing Influence on the Roughness and Microshear Bond Strength of a Lithium Silicate Glass-Ceramic for Laminate Veneers
Table 2
Means and standard deviations for dentin roughness parameters.
| Groups | Dentin roughness parameters (m) | | | |
| G1 | 0.10 ± 0.03 | 0.62 ± 0.14 | 0.12 ± 0.04 | G2 | 3.35 ± 0.39 | 16.31 ± 1.97 | 4.15 ± 0.52 | G3 | 1.48 ± 0.28 | 7.12 ± 1.07 | 1.78 ± 0.32 | G4 | 3.53 ± 0.68 | 16.27 ± 3.36 | 4.29 ± 0.82 | G5 | 2.07 ± 0.19 | 10.52 ± 0.90 | 2.65 ± 0.32 | G6 | 1.91 ± 0.27 | 9.08 ± 1.59 | 2.35 ± 0.35 | G7 | 1.58 ± 0.17 | 7.51 ± 0.87 | 1.90 ± 0.21 |
|
|
Values followed by the same letters in column are statistically similar ().
|