Consecutive hydrogenation of allyl alcohol portions in the presence of (1) poly-PdAAm/SiO2 and (2) poly-PdAAm/Al2O3. Initial substrate amount is 2.58 mmol; catalyst sample weight is 0.03 g; solvent: 20 mL of ethanol; temperature: 40°C.