Research Article

Preliminary Assessment of Oxidation Pretreated Hastelloy as Hydrocarbon Steam Reforming Catalyst

Figure 11

Scanning electron micrograph and EDX analysis of (a) unoxidized Hastelloy and (b) Hastelloy oxidized at 1000°C for 2 h.
210371.fig.0011a
(a)
210371.fig.0011b
(b)