Transition in Deformation Mechanism of AZ31 Magnesium Alloy during High-Temperature Tensile Deformation

Figure 12

The slip morphology on the specimen surface after 40% tensile deformation at a strain rate of  s−1 and a temperature of 573 K.
165307.fig.0012a
(a)
165307.fig.0012b
(b)

We are committed to sharing findings related to COVID-19 as quickly and safely as possible. Any author submitting a COVID-19 paper should notify us at help@hindawi.com to ensure their research is fast-tracked and made available on a preprint server as soon as possible. We will be providing unlimited waivers of publication charges for accepted articles related to COVID-19. Sign up here as a reviewer to help fast-track new submissions.