Research Article

Fabrication of Single-Phase NiTi by Combustion Synthesis of Mechanically Activated Powders

Figure 6

SEM images of the Ni-Ti powder mixture after milling for 5 h: (a) 1000X, (b) 5000X.
153841.fig.006a