Research Article

Heat Treatment in High Chromium White Cast Iron Ti Alloy

Figure 12

Effect of austenitizing temperature, applied load, and Ti-addition on abrasion wear rate of the investigated alloys treated at (a) 1150°C and (b) 980°C.
856408.fig.0012a
(a)
856408.fig.0012b
(b)