X-ray diffraction results for the investigated alloys.
| d-spacing (Å) | Intensity (%) | | Phase |
| 2.036 | 45.6 | 0.1431 | Carbide | 2.011 | 17.6 | 0.1431 | Carbide | 2.080 | 62.0 | 0.1372 | Austenite | 1.268 | 2.8 | 0.3687 | Eutectic austenite | 2.073 | 40.7 | 0.1379 | Eutectic austenite | 0.827 | 2.6 | 0.8677 | Eutectic austenite | 0.904 | 3.2 | 0.7278 | Austenite |
|
|