Variation of (a) sulphur content and (b) desulfurization degree of the metal using 250 gm of CaO-CaF2 (4 : 1) in the furnace and adding 250 gm of different types of flux in the mold: (1) CaO + CaF2, (2) Na2CO3, (3) CaO + CaF2 + Al2O3, (4) CaO + CaF2 + FeSi + C, and (5) CaSi.