Mill scale experimental runs (reducing agent: coke).
| Heat number | Stoichiometric carbon | Chemical composition of produced metal, wt% | C | Si | Mn | S | P |
| 1 | 0.9 | 0.02 | 0.001 | 0.032 | 0.199 | 0.005 | 2 | 1.0 | 0.32 | 0.004 | 0.127 | 0.210 | 0.015 | 3 | 1.1 | 1.80 | 0.005 | 0.171 | 0.191 | 0.018 | 4 | 1.2 | 1.81 | 0.008 | 0.122 | 0.151 | 0.015 | 5 | 1.3 | 3.04 | 0.020 | 0.211 | 0.165 | 0.022 | 6 | 1.5 | 3.84 | 0.079 | 0.337 | 0.053 | 0.015 | 7 | 1.6 | 3.13 | 0.664 | 0.495 | 0.067 | 0.016 | 8 | 1.7 | 3.74 | 0.969 | 0.675 | 0.021 | 0.015 |
|
|